INSPECTING & FIRING

At this stage, a careful inspection is made of the investment to make sure no cracks have appeared in the shell.

Any cracks are sealed over with a ceramic putty.

 

After the investment passes inspection, it is fired in the kiln at approx 950°C for one hour to strengthen the shell to the point where it can withstand the heat and pressure of molten bronze.